防水补漏方法 |
添加时间:2019/7/31 15:02:12 浏览次数: |
堵漏堵漏 Leakage plugging 用凿子或冲击钻将渗水部位打成4~5cm深,直径2~3cm的孔洞,用于冲洗干净后,r-1型材料加水(灰:水=1:0.3)搅拌均匀,捏成料团(料团大小与孔洞相近),手掌感觉发热,迅速将料团塞于孔中,并用手掌压住几分钟,手掌感到发硬后,松开手掌,再用木板压平。15min后进行湿养护。 防水堵漏 Drill the seepage into 4-5 cm deep hole with a chisel or percussion drill. After rinsing, mix the R-1 material with water (ash: water = 1:0.3), knead the material into a ball (the size of the material ball is similar to the hole), feel the heat in the palm, quickly plug the material into the hole, and press the material into the palm for a few minutes, and feel the hair in the palm. After hardening, loosen your palms and press them flat with boards. After 15 minutes, wet maintenance was carried out. Waterproof and leak stoppage 抹面抹面 Apply the face 基面清理干净,充分湿润后,r-1型材料加水(灰:水=1:0.4)搅拌均匀(不得含生料或团粒)成腻子状,用抹子或刮板迅速上第一层料(厚度1mm),涂层硬化后喷水湿养护,再上第二层料(厚度1mm),上料时稍用力使涂层密实。若还有局部渗水或有湿渍,只需在渗水或湿渍部位再加涂一层,直到不渗不湿。并注意搭接,每次配料不要太多(每次搅拌应在凝结前用完),以免造成浪费。涂层硬化后要进行湿养护3d。 After the base surface is cleaned and fully wetted, the R-1 material is mixed with water (ash: water = 1:0.4) evenly (no raw materials or aggregates) to form putty. The first layer (thickness 1 mm) is quickly coated with a plaster or scraper. After hardening, the coating is wet cured by spraying water, and then the second layer (thickness 1 mm) is coated with a little force to make the coating dense. If there is local water seepage or wetting, just add another layer to the water seepage or wetting area until it is not wet. And pay attention to lapping, not too much ingredients (each mixing should be used up before condensation), in order to avoid waste. After hardening, the coating should be wet cured for 3 days. |
上一页 防水补漏基本知识 |
下一页 楼层及厕浴、厨房间防水补漏的方法 |
Copyright © 技术支持:遨游网络